Differential Scanning Calorimetry (DSC)
Capabilities: Phase transitions detection, glass transition & crystalline melt of polymers.
Equipment Make: TA Instruments
Equipment Model: Q20
Problems addressed:Thermal analysis of polymers, Af/Mf detection in Nitinol.
Advantages: Quick analysis, small sample size (10mg).